Paper
Paper
Search...
Search ResearchHub...
Ctrl+K
New
Home
Browse
Earn
Fund
RH Journal
Notebook
Lists
Leaderboard
RSC
USD
Changelog
Terms
Privacy
Issues
Docs
Support
Foundation
About
Stress Corrosion Cracking of Austenitic Stainless Stesls ... | ResearchHub
Paper
Paper
Search...
Search ResearchHub...
Ctrl+K
New
Home
Browse
Earn
Fund
RH Journal
Notebook
Lists
Leaderboard
RSC
USD
Changelog
Terms
Privacy
Issues
Docs
Support
Foundation
About
Stress Corrosion Cracking of Austenitic Stainless Stesls in Chemical Plants and Related Preventive Measures, Especially Application of Ferritic Stainless Steels
0
Authors
Katsumi Yamamoto
1 more
Katsumi Yamamoto
•
Naohiko Kagawa
Published
March 3, 1980
Paper
Conversation
0
Reviews
0
Bounties
0
Sign in to comment
Add a comment...
Best
Supporters
Support the authors with ResearchCoin
Tip RSC
Journal
CORROSION
Topics
Materials Science
Materials Chemistry
Metals And Alloys
Stress (Linguistics)
Composite Material
Show all topics
DOI
10.5006/c1980-80092